pb_paulie_b said:What did you use? Cloudiness is common with this piece. It because of the sad quality of the metal.
Here's one that I did...PB
pb_paulie_b said:It because of the sad quality of the metal.
I beg to differ. It's basicly pot metal. The cheappest of the cheap.Cougar5.O said:These sort of surface imperfections are common in casting grade aluminum that has a lot of impurities added to aid in flow (filling the casting) & release from the casting (lubricants). It is in no way indicative of the quality of the metal.
pb_paulie_b said:I beg to differ. It's basicly pot metal. The cheappest of the cheap.
Then you already know it's cheap.Cougar5.O said:Well, I design castings for a living so maybe I do know about casting grade aluminum.
pb_paulie_b said:Then you already know it's cheap.